MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LyondellBasell CirculenRecover C14 HP640J Polypropylene
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: CirculenRenew C14 HP640J is part of the Circulen product family of circular and sustainable solutions. CirculenRenew C14 HP640J polymer reduces the carbon footprint as it replaces fossil feedstock through using renewable raw material made from bio-based waste and residue oils. The renewable content of CirculenRene C14 is measured by an accredited third party laboratory and stated as a parameter on the certificate of analysis (CoA). CirculenRenew C14 HP640J is a drop-in solution and therefore doesn't require any adaptation of the existing processing equipment. CirculenRenew C14 HP640J is a nucleated homopolymer for extrusion and thermoforming applications. CirculenRenew C14 HP640J exhibits a good stiffness and transparency. The main applications of CirculenRenew C14 HP640J are fruit baskets, trays, transparent drinking cups and containers.

Status: Commercial - Active

Availability: Africa-Middle East; Europe

Application: Clear Containers; Thermoformed Food Containers

Market: Rigid Packaging

Processing Method: Sheet and Profile Extrusion; Thermoforming

Attribute: Homopolymer; Medium Stiffness; Medium Transparency; Nucleated

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 1183-1
Melt Flow 3.20 g/10 min
@Load 2.16 kg,
Temperature 230 °C
3.20 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 78.0 MPa11300 psiH 358/30; ISO 2039-1
Tensile Strength, Yield 37.0 MPa5370 psiISO 527-1, -2
Elongation at Break >= 50.0 %>= 50.0 %ISO 527-1, -2
Elongation at Yield 9.00 %9.00 %ISO 527-1, -2
Tensile Modulus 1.60 GPa232 ksiISO 527-1, -2
Charpy Impact, Notched 0.700 J/cm²3.33 ft-lb/in²Type 1, Edgewise, Notch A; ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C194 °FUnannealed; ISO 75B-1, -2
Vicat Softening Point 154 °C309 °FA50; ISO 306
 
Optical PropertiesMetricEnglishComments
Haze 30.0 %
@Thickness 0.991 mm
30.0 %
@Thickness 0.0390 in
ASTM D1003
Gloss 113 %113 %60°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQS9077 / 324012

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.