Celanese Celanex® 1602Z PBT, Unfilled
Categories:
Polymer
;
Thermoplastic
;
Polyester, TP
;
Polybutylene Terephthalate (PBT)
Material Notes:
Celanex 1602Z is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 1602Z has an internal lubricant.
Information provided by Celanese
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.31
g/cc
1.31
g/cc
ASTM D792
Density
1.31
g/cc
0.0473
lb/in³
ISO 1183
Water Absorption
0.080 %
@Temperature 22.8 °C
0.080 %
@Temperature 73.0 °F
24hr immersion; ASTM D570
Linear Mold Shrinkage, Flow
0.018
-
0.020
cm/cm
0.018
-
0.020
in/in
ISO 294-4
0.020
cm/cm
0.020
in/in
ASTM D955
Melt Flow
13
g/10 min
13
g/10 min
ASTM D1238
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell M
72
72
ISO 2039-2
Tensile Strength at Break
51.7
MPa
7500
psi
ASTM D638
Tensile Strength, Yield
60.0
MPa
8700
psi
50mm/min; ISO 527-2/1A
Tensile Stress at Strain
28.0
MPa
@Strain 50 %
4060
psi
@Strain 50 %
ISO 527-2/1A
Elongation at Break
>= 50 %
>= 50 %
200 %
200 %
ASTM D638
Elongation at Yield
5.0 %
5.0 %
50mm/min; ISO 527-2/1A
Tensile Modulus
2.55
GPa
370
ksi
50mm/min; ISO 527-2/1A
Flexural Strength
80.0
MPa
11600
psi
ISO 178
82.7
MPa
12000
psi
ASTM D790
Flexural Modulus
2.20
GPa
319
ksi
ISO 178
2.28
GPa
330
ksi
ASTM D790
Izod Impact, Notched
0.534
J/cm
1.00
ft-lb/in
ASTM D256
Izod Impact, Notched (ISO)
5.50
kJ/m²
2.62
ft-lb/in²
ISO 180/1A
Charpy Impact Unnotched
NB
NB
ISO 179/1eU
21.0
J/cm²
@Temperature -30.0 °C
99.9
ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched
0.700
J/cm²
3.33
ft-lb/in²
ISO 179/1eA
0.650
J/cm²
@Temperature -30.0 °C
3.09
ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
Electrical Properties
Metric
English
Comments
Volume Resistivity
>=
1.00e+15
ohm-cm
>=
1.00e+15
ohm-cm
IEC 60093
1.00e+16
ohm-cm
1.00e+16
ohm-cm
ASTM D257
Surface Resistance
>=
1.00e+15
ohm
>=
1.00e+15
ohm
IEC 60093
Dielectric Constant
3.24
@Frequency 1000 Hz
3.24
@Frequency 1000 Hz
ASTM D150
3.5
@Frequency 1e+6 Hz
3.5
@Frequency 1e+6 Hz
IEC 60250
4.0
@Frequency 100 Hz
4.0
@Frequency 100 Hz
IEC 60250
Dielectric Strength
15.7
kV/mm
400
kV/in
short term; ASTM D149
23.0
kV/mm
584
kV/in
IEC 60243-1
Dissipation Factor
0.0010
@Frequency 1000 Hz
0.0010
@Frequency 1000 Hz
ASTM D150
0.0014
@Frequency 100 Hz
0.0014
@Frequency 100 Hz
IEC 60250
0.021
@Frequency 1e+6 Hz
0.021
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index
600
V
600
V
IEC 60112
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
110
µm/m-°C
61.1
µin/in-°F
ISO 11359-2
Melting Point
225
°C
437
°F
10°C/min; ISO 11357-1,-2,-3
225
°C
437
°F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi)
150
°C
302
°F
ISO 75-1, -2
154
°C
310
°F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
50.0
°C
122
°F
ISO 75-1, -2
54.4
°C
130
°F
ASTM D648
Flammability, UL94
HB
HB
HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
Processing Properties
Metric
English
Comments
Processing Temperature
65.0
-
93.0
°C
149
-
199
°F
cavity
250
-
260
°C
482
-
500
°F
hot runner
Feed Temperature
230
-
240
°C
446
-
464
°F
Zone 1
230
-
240
°C
446
-
464
°F
Zone 2
235
-
250
°C
455
-
482
°F
Zone 3
235
-
250
°C
455
-
482
°F
Zone 4
240
-
260
°C
464
-
500
°F
Die Temperature
250
-
260
°C
482
-
500
°F
Melt Temperature
243
°C
469
°F
ISO 294
235
-
260
°C
455
-
500
°F
Mold Temperature
82.0
°C
180
°F
ISO 294
Injection Velocity
300
mm/sec
11.8
in/sec
ISO 294
Drying Temperature
120
-
130
°C
248
-
266
°F
Dry Time
4.00
hour
4.00
hour
Moisture Content
<= 0.020 %
<= 0.020 %
Hold Pressure
48.0
MPa
6960
psi
ISO 294
Descriptive Properties
Injection molding
Yes
Injection speed
medium-fast
Processing conditions acc. ISO
7792-2
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Celanese Celanex® 1500A PBT, Unfilled
Celanese Celanex® 1400FC PBT, Unfilled
Celanese Celanex® 1462Z PBT, 30% Glass Reinforced
Celanese Celanex® 2000-3 PBT, Unfilled
Celanese Celanex® 2000-3FC PBT, Unfilled
PHCQ007 / 178462
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.