MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Radici RADIPOL® 45A00D Nylon 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: N° CAS. 32131-17-2

Description: Polyamide 66, Standard viscosity, Dry, Brightly

Typical Applications: Base polymer for melt spinning BCF

Information provided by Radici Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ISO1183
Viscosity  50000 cP
@Shear Rate 3000 1/s,
Temperature 290 °C
50000 cP
@Shear Rate 3000 1/s,
Temperature 554 °F
Apparent shear
 60000 cP
@Shear Rate 1000 1/s,
Temperature 290 °C
60000 cP
@Shear Rate 1000 1/s,
Temperature 554 °F
Apparent shear
 70000 cP
@Shear Rate 70.0 1/s,
Temperature 290 °C
70000 cP
@Shear Rate 70.0 1/s,
Temperature 554 °F
Apparent shear
Viscosity Measurement 2.72.7Relative, Solvent: sulphuric acid 95.7%; Polyamide concentration:0.01 g/ml
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °FScanning rate 10°C/min; ISO 11357-1-3
 
Optical PropertiesMetricEnglishComments
Yellow Index <= -6.00 %<= -6.00 %
 
Descriptive Properties
Amino End Group46 meq/kgMA0014
Carboxylic end group73 meq/kgMA0014
Chip Size2.0x2.5x3.0 mm
ColorNatural
Granulometry1.9 g/100 chips

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRADICI018 / 313519

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.