MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Phillips 66 C-3 Hydraulic Transmission Fluid, Type C-3
Categories: Fluid; Lubricant

Material Notes: Description: Conoco Hydraulic Transmission Fluid, Type C-3 is a heavy-duty, low viscosity fluid for mobile hydraulic systems, torque converters and automatic transmissions. Use it in Allison powershift transmissions and other transmissions that require an Allison C-3, C-2 or C-1 fluid. Common applications include off-highway construction equipment, haul trucks, motor graders, scrapers, farm tractors, cranes, shovels and rollers. Hydraulic Transmission Fluid, Type C-3 offers excellent rust and corrosion protection and wear control. It resists foaming and circulates well, even in low temperatures.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 32.6 °
Viscosity Measurement 121Viscosity Index
Kinematic Viscosity at 40°C (104°F) 31.2 cSt
Kinematic Viscosity at 100°C (212°F) 6.5 cSt
ASTM Color 1.5
 
Thermal PropertiesOriginal ValueComments
Pour Point -22.0 °F
Flash Point 441 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON010 / 75047

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.