MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

HB Fuller Swift®therm 2699 Polyolefine Hot Melt
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: Type of Product: Hot melt

Product Benefits:

  • High green strength
  • Good bonding at elevated temperature
  • Especially suitable for polar and nonpolar surfaces
  • High softening point
  • Low viscosity for easy application and good wetting of substrates
Typical Applications: Automotive interior trim

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.920 g/cc0.920 g/cc
Brookfield Viscosity 12500 cP
@Temperature 177 °C
12500 cP
@Temperature 351 °F
10 1/min, Sp. 27
 
Thermal PropertiesMetricEnglishComments
Ring & Ball Softening Point 155 °C311 °FDIN EN 1427
 
Processing PropertiesMetricEnglishComments
Processing Temperature 165 - 185 °C329 - 365 °F
 
Descriptive Properties
Base compoundThermoplastic polyolefine
ColorLight-amber
ConsistencySolid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHBFULL082 / 316873

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.