MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Free-Cutting Brass, UNS C36000, Annealed Rod
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Fair to excellent corrosion resistance. Excellent machinability. Fabricated by machining, roll threading and knurling.

Applications: gears, pinions, automatic high-speed screw machine parts.

Test specimen: Rod cold drawn 30% to 19 mm (0.75 in) diameter then annealed 1 hour. Initial tensile strength before annealing 490 MPa (70,000 psi).

Key Words: free cutting, FC, CDA 360, CZ124, ISO CuZn36Pb3, CEN CW603N, FED QQ-B-626 (discontinued), ASTM-B121, ASTM-B36, ASTM-B16/B16M, ASTM-B124
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.50 g/cc
Grain Size 9.0 µm
@Treatment Temp. 350 °C
 9.0 µm
@Treatment Temp. 400 °C
 13 µm
@Treatment Temp. 500 °C
 20 µm
@Treatment Temp. 600 °C
 31 µm
@Treatment Temp. 700 °C
 52 µm
@Treatment Temp. 800 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 325 MPa
@Treatment Temp. 800 °C
 330 MPa
@Treatment Temp. 700 °C
 345 MPa
@Treatment Temp. 600 °C
 375 MPa
@Treatment Temp. 500 °C
 425 MPa
@Treatment Temp. 400 °C
 475 MPa
@Treatment Temp. 300 °C
 490 MPa
@Treatment Temp. 200 °C
Elongation at Break 13 %
@Treatment Temp. 200 °C
 20 %
@Treatment Temp. 300 °C
 33 %
@Treatment Temp. 400 °C
 40 %
@Treatment Temp. 500 °C
 54 %
@Treatment Temp. 800 °C
 55 %
@Treatment Temp. 600 °C
 56 %
@Treatment Temp. 700 °C
Modulus of Elasticity 97.0 GPa
Poissons Ratio 0.311
Machinability 110 %Excellent - the standard against which other copper alloys are judged
Shear Modulus 37.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000660 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 20.5 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.380 J/g-°C
Thermal Conductivity 115 W/m-K
@Temperature 20.0 °C
Melting Point 885 - 900 °C
Solidus 885 °C
Liquidus 900 °C
Annealing Point 800 - 1100 °F
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 425 - 600 °C
Hot-Working Temperature 700 - 800 °C
Recrystallization Temperature 330 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 60 - 63 %
Iron, Fe <= 0.35 %
Lead, Pb 2.5 - 3.7 %
Other, total <= 0.50 %
Zinc, Zn 35.5 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Free-Cutting Brass, UNS C36000
Free-Cutting Brass, UNS C36000, H01 (Cold Drawn 15%) Temper shapes
Mueller Alloy 3600 Free Cutting Brass (UNS C36000)
Free-Cutting Brass, UNS C36000, H02 (Cold Drawn 25%) Temper 6 mm rod
Free-Cutting Brass, UNS C36000, H02 (Cold Drawn 20%) Temper 25 mm rod

MC36000c1 / 171650

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.