MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Samyang Tramid® 210G45 Polyamide, Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.
210G45 is a reinforced grade.

Applications:

  • Automotive gear level housing
  • Connectors
  • Intake manifolds
  • Thermostat housing
  • Cooling radiator modules
  • Sprinkler
  • Water pipes
  • Fan and shroud
  • ECU cases
  • Cylinder head cover
  • Industrial ball valve

Information provided by Samyang.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.51 g/cc1.51 g/ccASTM D792
Water Absorption 0.50 %0.50 %ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 226 MPa32700 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
Flexural Yield Strength 299 MPa43400 psiASTM D790
Flexural Modulus 11.5 GPa1660 ksiASTM D790
Izod Impact, Notched 1.47 J/cm
@Thickness 3.17 mm
2.76 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 21.0 kV/mm533 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Melting Point 263 °C505 °FASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 254 °C489 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSANX971 / 133365

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.