MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger TECATEC PEI CW50 PL V01 natural Polyetherimide, Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyetherimide (PEI); Polyetherimide (PEI), Carbon Fiber Filled

Material Notes:
  • inherent flame resistance
  • good surface appearance
  • excellent mechanical properties
Target Industries:
  • automotive industry
  • mechanical engineering
  • oil and gas industry
  • safety engineering
  • sporting goods

Information provided by Ensinger Inc.

Vendors: Ensinger TECAPEI™ shapes combine Ultem® PEI polymer with Ensinger's proprietary extrusion techniques for exceptional reliability, consistency, dimensional stability, and high temperature mechanical performance. FDA, USP Class VI and NSF compliant.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.52 g/cc0.0549 lb/in³
Filler Content 50 %50 %Fiber volume
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 650 MPa94300 psiISO 527-4
Modulus of Elasticity 56.0 GPa8120 ksiISO 527-4
Flexural Strength 770 MPa112000 psiISO 14125
Flexural Modulus 46.0 GPa6670 ksiISO 14125
Compressive Strength 630 MPa91400 psiISO 14126
Compressive Modulus 52.0 GPa7540 ksiISO 14126
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 5.00 µm/m-°C2.78 µin/in-°F
CTE, linear, Transverse to Flow 5.00 µm/m-°C2.78 µin/in-°F
Maximum Service Temperature, Air 180 °C356 °Flong term
 200 °C392 °Fshort term
Glass Transition Temp, Tg 217 °C423 °F
 
Descriptive Properties
Colornatural
Fiber volume content (%)50
General material information0-90°Fiber orientation
 1-95 mmthickness
 200 g/m²Fiber areal weight
 345 g/m²Areal weight finished product
 625x525 mmMaterial widths
 carbon HT 3kFiber type
 twill 2/2Fiber architecture
Resin weight content (%)42.7

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIN8228 / 319156

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.