MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

Lucas-Milhaupt Silvacore® A38T Flux Cored Brazing Alloy
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes: Silvaloy A38T is used for joining ferrous metals, copper, copper alloys, nickel, nickel alloys and combinations of these metals. The tin content provides good wetting on many difficult to wet metals such as stainless steel and tungsten carbide. This alloy, being free of Pb or Cd is preferred for long heating cycles and is suitable for use in controlled atmosphere brazing without flux. The largest use of this alloys is the furnace brazing although it is also suitable for other brazing procedures.

Information provided by Lucas-Milhaupt Warwick, LLC (formerly Wolverine Joining Technologies).

Key Words: AWS BAg-34
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000950 ohm-cm0.00000950 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Melting Point 649 - 721 °C1200 - 1330 °F
Solidus 649 °C1200 °F
Liquidus 721 °C1330 °F
Maximum Service Temperature, Air 204 °C400 °Fcontinuous
 316 °C600 °Fintermittent
 
Processing PropertiesMetricEnglishComments
Processing Temperature 721 - 843 °C1330 - 1550 °FBrazing Temperature
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 31 - 33 %31 - 33 %Metal (excluding flux)
Other, total <= 0.15 %<= 0.15 %Metal (excluding flux)
Silver, Ag 37 - 39 %37 - 39 %Metal (excluding flux)
Tin, Sn 1.5 - 2.5 %1.5 - 2.5 %Metal (excluding flux)
Zinc, Zn 26 - 30 %26 - 30 %Metal (excluding flux)
 
Descriptive Properties
Boric Acid %27percentage of flux
ColorPale Yellow
Electrical Conductivity (% IACS)18
Potassium Bifluoride %27percentage of flux
Potassium Fluoroborate %25percentage of flux
Potassium Tetraborate %21percentage of flux

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lucas-Milhaupt BRAZE 999 Commercial Grade Fine Silver
Lucas-Milhaupt Cerametil 616 Active Metal Brazing
Lucas-Milhaupt Silvaloy® A20 Brazing Alloy
Overview of materials for Silver Alloy
Johnson Matthey Mattibraze™ 35 Silver Brazing Alloy - Cadmium Bearing

NBRW028 / 79804

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.