MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LG Chemical LUPOS HR-2307 Heat Resistant SAN, 30% Glass Fiber Reinforced  (discontinued **)
Categories: Polymer; Thermoplastic; SAN Polymer; Styrene Acrylonitrile (SAN), Molded, Glass Reinforced

Material Notes: LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have a wide range of applications in automotive parts, electrical/electronic parts. and industrial equipments, etc.

Applications:

    Automotive: Main core, glove box, meter box, head lamp housing, back mirror cover, etc.

    Electrical and Electronic: Computer tape reel, pan cake hub for video and audio, stereo speaker box, fan for air conditioner, washing machine pulley, fax frame

    Others:Camera body, fishing reel, bobbin

Information Provided by LG Chem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.40 g/ccASTM D792
Linear Mold Shrinkage 0.0010 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.0020 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 127 MPaASTM D638
Elongation at Break 5.0 %ASTM D638
Flexural Strength 155 MPaASTM D790
Flexural Modulus 9.02 GPaASTM D790
Izod Impact, Notched 39.0 J/m
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 108 °CASTM D648
Flammability, UL94 HB
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 210 - 230 °C
Middle Barrel Temperature 220 - 240 °C
Front Barrel Temperature 230 - 250 °C
Nozzle Temperature 230 - 250 °C
Melt Temperature 240 - 260 °C
Mold Temperature 60.0 - 90.0 °C
Drying Temperature 90.0 °C
Dry Time 3 - 4 hour
Injection Pressure 78.45 - 88.26 MPaSecond
 68.65 - 98.07 MPaFirst
Back Pressure 0.000 - 3.92 MPa
Screw Speed 40 - 60 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MetalTek HAYNES® HR120 Severe Corrosion and Heat Resistant Alloy
MetalTek HAYNES® 230 Severe Corrosion and Heat Resistant Alloy
LG Chemical LUPOS GP2305A SAN+GF30%, General Purpose
Ineos ABS Lustran® SAN GF30 Glass Fiber Reinforced
Haynes HR-160® alloy, solution annealed sheet

PLGCHEM110 / 50931

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.