MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NeoGraf GRAFOIL® GHR Standard Fluid Sealing Laminate, Metal Reinforced
Categories: Carbon; Graphite

Material Notes: GRAFOIL® Grade GHR is an uncured laminate made with GRAFOIL® Grade GTB flexible graphite adhesively bonded to both faces of a 0.002" thick flat 316 or 316L stainless steel insert. Surface identifiable, the laminate is branded with the GRAFOIL® grade and source guarantee. Grade GHR is suitable for standard industrial fluid sealing applications as well as applications in: chemical, petrochemical, refinery, steam service, cryogenic, and ASME class 150 & 300 flanges. While maintaining an effective seal, GRAFOIL® material exhibits virtually no creep relaxation. As a result, the need for periodic bolt tightening is greatly reduced. Laminate Construction: GRAFOIL® Grade GTB ? 0.002" thick flat 316 or 316L stainless steel (per ASTM F-A-240 and AMS 5524) ? GRAFOIL® Grade GTB

Formerly a product of GrafTech.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 1.12 g/cc0.0405 lb/in³Standard; Graphite
Thickness 810 microns31.9 milStandard; Laminate
 1570 microns61.8 milStandard; Laminate
 3100 microns122 milStandard; Laminate
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 26.2 MPa3800 psiadditive of steel and GRAFOIL® flexible graphite
Compression Set 85 %
@Pressure 34.5 MPa
85 %
@Pressure 5000 psi
after 5000 psi load
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 525 °C977 °F
Minimum Service Temperature, Air -240 °C-400 °F
 
Descriptive Properties
"m" Factor2ASME Gasket Factor
"y" Stress (psi)900ASME Gasket Factor
Compressibility (%)40at 5000 psi load
Max Gasket Unit Load (psi)24000ASME Gasket Factor
Resistance in #1 Oil (%)<33Weight change
 <8Thickness increase
Resistance in #3 Oil (%)<12Thickness increase
 <35Weight change

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chosun Refractories CAR-1 Carbon Brick
NeoGraf eGRAF® HITHERM™ HT-720 Graphite
NeoGraf eGRAF® SPREADERSHIELD™ SS600 Graphite
UCAR Carbon UCAR® ATA Isostatic Molded Graphite
Aremco Pyro-Paint™ 634-CA High Temperature Refractory Coating

CGRAF940 / 107344

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.