MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
TOSAF Compounds Tosaf MP800121 PP, Masterbatch
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Product Description: MP800121 is suitable for coloring of molded and extruded articles made of various types of Polypropylene.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Agency Ratings: BfR IX; EN 71-3; EU 10/2011; FDA 21 CFR 178.3297

RoSH Compliance: RoSH Compliant

Additives Category: Masterbatch – Pigment – White

Carrier Resin: Polypropylene or propylene-olefin copolymer (PP)

Recommended for Use In: Polypropylene or propylene-olefin copolymer (PP)

White Pigment Composition (<80%): Titanium dioxide (TiO2)

Chemical Description: Titanium dioxide

State at Room Temperature: Solid

Information provided by TOSAF Compounds Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 25 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Thermal PropertiesOriginal ValueComments
Melting Point 284 - 338 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 536 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTOSAF1509 / 312202

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.