Symbol according to ISO 1043/1: PC+ABS Unfilled. Suitable for Injection Molding. Supplied as pellets. ISO data. Information provided by Enichem Versalis is the Eni subsidiary containing the plastics and rubber businesses. |
Poly(Acrylonitrile Butadiene Styrene) + Polycarbonate |