MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Dow INNATE™ ST51 PE
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Product Description: INNATE ST 51 Precision Packaging Resin is designed for exceptional abuse performance. It offers a unique combination of high stiffness with excellent toughness which enables excellent performance on automated packaging equipment. This product also delivers robust processability.

Availability: North America

Additive: Antiblock: 3750 ppm; Processing Aid: No; Slip: No

Agency Ratings: EU 2011/10/EC; FDA 21 CFR 177.1520 ©3.2a

Form: Pellets

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.923 g/ccASTM D792
Melt Flow 0.85 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Antiblock Level 3750 ppm
 
Mechanical PropertiesOriginal ValueComments
Puncture Resistance 20.7 lb (f)
Film Tensile Strength at Yield, MD 1600 psiASTM D882
Film Tensile Strength at Yield, TD 1670 psiASTM D882
Film Elongation at Break, MD 450 %ASTM D882
Film Elongation at Break, TD 600 %ASTM D882
2% Secant Modulus 30500 psiMD; ASTM D8822
 34400 psiTD; ASTM D8822
Puncture Energy 54.9 in-lb
Elmendorf Tear Strength MD 650 gASTM D1922
Elmendorf Tear Strength TD 930 gASTM D1922
Dart Drop Test 1800 gMethod A; ASTM D1709
Film Tensile Strength at Break, MD 4280 psiASTM D882
Film Tensile Strength at Break, TD 5950 psiASTM D882
 
Optical PropertiesOriginal ValueComments
Haze 15 %ASTM D1003
Gloss 40 %45°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Blow-up Ratio (BUR) 2.5
 
Descriptive Properties
Film Puncture Resistance203 ft-lb/in3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWF547 / 311240

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.