MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Thermoseal

(Viewing data as-entered. Click here to return)
Klinger Thermoseal ML-N562 PTG Gasketing
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Thermoseal ML-N562 is a synthetic fiber and nitrile butadiene gasket material designed for difficult sealing applications with very low flange pressures or very rough surface finishes. It combines Multi-Layer Technology structure for exceptional low flange pressure sealability and exceptional torque retention together w ith a more compressible core. Multi-Layer Technology sheet products consist of a reinforced high density core w ith conformable sealing layers on each side. ML-N562 provides heat and chemical resistance in coolant, lubricant, and hot air applications. Typical applications include automotive, marine, and small engine applications with intermittent operating temperatures up to 500° F (260° C).

Information provided by Thermoseal Inc.

Vendors: Thermoseal Inc. is the exclusive North American producer of Klinger Fluid Sealing products, including popular lines: Sealex, Klingersil and Topchem and our new Performance Technology Group of products. Visit us at Thermosealinc.com or call 1-800-990-7325 to speak with a fluid sealing specialist.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.40 g/ccASTM F1315
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 500 °Fintermittent
 
Descriptive Properties
ASTM F104 Line Call OutF715121B3E12K6M4
Compressibility>20%ASTM F36J
Creep<20%ASTM F38B (1/32")
Pressure<1400 psi
Recovery>50%ASTM F36J
Sealability<0.20 ml/hrASTM F37
Thickness Increase<10%After immersion in ASTM Oil #1 for 5 hrs at 300°F
 <15%After immersion in Fuel B for 5 hrs at 73°F
Weight Increase<10%After immersion in Fuel B for 5 hrs at 73°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Klinger Thermoseal ML-5270 PTG Gasketing
Klinger Thermoseal KLINGERSIL® C-4300 General Application Gasketing
Klinger Thermoseal KLINGERSIL® C-4201 General Application Gasketing
Klinger Thermoseal KLINGERSIL® C-4430 Compressed Inorganic Fiber Gasketing
Klinger Thermoseal KLINGERSIL® C-8200 Chemical Resistant Gasketing

PTHERM930 / 150417

Thermoseal

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.