MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lubrizol Advanced Materials PEARLTHANE® D11H92S Thermoplastic Polyurethane Elastomer
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: PEARLTHANE® D11H92S is a high performance polycaprolactone copolyester based TPU, supplied in form of translucent, colorless pellets, featuring excellent flow and mechanical properties and an outstanding low compression set value and high temperature resistance. Product recommended for injection-molding applications with an extremely short cycle time.

All information provided by Merquinsa

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/ccISO 2781
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9292ISO 868
Hardness, Shore D 9292ISO 868
Tensile Strength, Yield 46.00 MPa6672 psiISO 527-2/5A/500
Elongation at Break 460 %460 %ISO 527-2/5A/500
100% Modulus 10.0 MPa
@Strain 100 %
1450 psi
@Strain 100 %
ISO 527-2/5A/500
300% Modulus 21.00 MPa
@Strain 300 %
3046 psi
@Strain 300 %
ISO 527-2/5A/500
Tear Strength 125 kN/m713 pliUnnicked; ISO 34-1B
Abrasion 2020Resistance, [mm3]; ISO 4649
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 133 °C271 °FUnannealed; ISO 306 (A50)
 139 °C282 °FAnnealed; ISO 306 (A50)
 
Processing PropertiesMetricEnglishComments
Feed Temperature 40.0 °C104 °F
Nozzle Temperature 200 °C392 °F
Zone 1 190 °C374 °F
Zone 2 195 °C383 °F
Zone 3 195 °C383 °F
Zone 4 195 °C383 °F
Drying Temperature 90.0 °C
@Time 10800 sec
194 °F
@Time 3.00 hour
Dew Point <= -30.0 °C<= -22.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Advanced Materials Pearlthane® 12H92E Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® 11T92EM Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® 11H98 Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® 15N95UV Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® Clear 15N85 Thermoplastic Polyurethane Elastomer

PMES36a / 109240

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.