MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Schmolz + Bickenbach UGIMA® 303 Stainless Steel Bar
Categories: Metal; Ferrous Metal; Stainless Steel; T 300 Series Stainless Steel

Material Notes: 303 UGIMA® is Ugitech’s improved machining grade produced only by Ugitech. It is identical in every way to regular 303, except with respect to machinability. 303 UGIMA® represents Ugitech's popular UGIMA® family of high machinability grades. Through the use of new and beneficial modifications to the steel-making process, 303 UGIMA® builds upon the proprietary UGIMA® manufacturing process to allow for excellent machinability across a wider range of operations and cutting conditions. When compared with older versions, 303 UGIMA® is a technologically advanced product that will allow for superior machinability at both low and high speeds, in cam-driven and CNC machines, and with high-speed steel or carbide tooling. Machine shops using 303 UGIMA® have experienced consistent success regardless of machine, operation, tooling, or cutting conditions. From lot to lot, 303 UGIMA® is engineered to give the same high performance every time without surprises.

Applications: Fasteners, Shafts, Valve Bodies, Valves, Valve Trim, Fittings, Machined parts, and Not recommended for vessels containing liquid or gasses at high pressures

Information provided by Schmolz + Bickenbach

Key Words: AISI 303; UNS S30300; EN 10088-3 1.4305; X8CrNiS 18-8; SAE J405; ASTM A314; ASTM A320 Class 1; A484; A581; A582; F899; AMS 5640 Type 1; QQ-S-763C; QQ-S_764B, Amend 2; MIL-S-862; MIL-W-52263C
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.89 g/cc0.285 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 220 - 240220 - 240Escomatic Coils
 170 - 190
@Thickness >=25.4 mm
170 - 190
@Thickness >=1.00 in
Turned Bars
 220 - 240
@Thickness <=25.4 mm
220 - 240
@Thickness <=1.00 in
Cold Drawn Bars
Tensile Strength 655 - 827 MPa95000 - 120000 psiEscomatic Coils
 586 - 689 MPa
@Thickness >=25.4 mm
85000 - 100000 psi
@Thickness >=1.00 in
Turned Bars
 655 - 827 MPa
@Thickness <=25.4 mm
95000 - 120000 psi
@Thickness <=1.00 in
Cold Drawn Bars
Tensile Strength, Yield 483 - 689 MPa
@Strain 0.2 %
70000 - 100000 psi
@Strain 0.2 %
Escomatic Coils
 241 - 379 MPa
@Strain 0.2 %,
Thickness >=25.4 mm
35000 - 55000 psi
@Strain 0.2 %,
Thickness >=1.00 in
Turned Bars
 483 - 689 MPa
@Strain 0.2 %,
Thickness <=25.4 mm
70000 - 100000 psi
@Strain 0.2 %,
Thickness <=1.00 in
Cold Drawn Bars
Elongation at Yield >= 30 %>= 30 %Escomatic Coils
 >= 30 %
@Thickness <=25.4 mm
>= 30 %
@Thickness <=1.00 in
Cold Drawn Bars
 >= 50 %
@Thickness >=25.4 mm
>= 50 %
@Thickness >=1.00 in
Turned Bars
Reduction of Area >= 45 %>= 45 %Escomatic Coils
 >= 45 %
@Thickness <=25.4 mm
>= 45 %
@Thickness <=1.00 in
Cold Drawn Bars
 >= 60 %
@Thickness >=25.4 mm
>= 60 %
@Thickness >=1.00 in
Turned Bars
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000730 ohm-cm0.0000730 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.7 µm/m-°C
@Temperature 20.0 - 200 °C
9.30 µin/in-°F
@Temperature 68.0 - 392 °F
Thermal Conductivity 15.3 W/m-K
@Temperature 20.0 °C
106 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 1010 - 1090 °C1850 - 2000 °FFollowed by rapid cooling with forced air or water quenching
Hot-Working Temperature 954 - 1200 °C1750 - 2200 °FForging range
 1180 - 1200 °C2150 - 2200 °FHeat in range
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.15 %<= 0.15 %
Chromium, Cr 17 - 19 %17 - 19 %
Copper, Cu <= 1.0 %<= 1.0 %
Iron, Fe 65.9 - 69.9 %65.9 - 69.9 %
Manganese, Mn <= 2.0 %<= 2.0 %
Molybdenum, Mo <= 0.60 %<= 0.60 %
Nickel, Ni 8.0 - 10 %8.0 - 10 %
Phosphorus, P <= 0.20 %<= 0.20 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S >= 0.15 %>= 0.15 %
 
Descriptive Properties
Corrosion ResistanceAcetic Acid2/4
 Humidity3/4
 NaCl (Saline Mist)2/4
 Nitric Acid3/4
 Phosphoric Acid2/4
 Sodium Carbonate2/4
 Sulfuric Acid2/4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
303 Stainless Steel, annealed
AISI 303 Cast Stainless Steel, ASTM A582
AISI 303 Cast Stainless Steel, EN 10088
AISI 303 Cast Stainless Steel, UNS J92511
Schmolz + Bickenbach UGIMA® 303 HD Stainless Steel Bar

NSCHMO031 / 125904

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.