MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Copper Alloy, UNS C70315, STOL 94, TM01 Temper, Strip, Sheet, Rod, Bar
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Mill-hardened Temper, TM - 1/2 Hard

Fabrication Properties: Excellent Suitability – Capacity for Being Hot Formed; Good Suitability – Soldering, Brazing, Gas Shielded Arc Welding, Capacity for Being Cold Worked; Fair Suitability – Spot Weld, Seam Weld, Butt Weld

Typical uses: Electrical Connectors – Automotive; Connector Components

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.86 g/cc0.320 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 180 - 240
@Load 3.00 kg
180 - 240
@Load 6.62 lb
Tensile Strength 621 - 717 MPa90000 - 104000 psi
Tensile Strength, Yield >= 538 MPa>= 78000 psi0.2% Offset
Elongation at Break 16 %16 %
Tensile Modulus 132 GPa19100 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000400 ohm-cm0.00000400 ohm-cm43% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.1 µm/m-°C
@Temperature 20.0 - 300 °C
9.50 µin/in-°F
@Temperature 68.0 - 572 °F
Thermal Conductivity 15.4 W/m-K107 BTU-in/hr-ft²-°F
Melting Point 1040 - 1060 °C1904 - 1940 °F
Solidus 1040 °C1904 °F
Liquidus 1060 °C1940 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 91.3 - 98.9 %91.3 - 98.9 %As Balance
Iron, Fe <= 0.10 %<= 0.10 %
Lead, Pb <= 0.050 %<= 0.050 %
Nickel, Ni 1.0 - 4.0 %1.0 - 4.0 %
Phosphorus, P <= 0.050 %<= 0.050 %
Silicon, Si 0.080 - 1.0 %0.080 - 1.0 %
Silver, Ag <= 0.50 %<= 0.50 %
Tin, Sn <= 1.0 %<= 1.0 %
Zinc, Zn <= 2.0 %<= 2.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC70315x7 / 292430

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.