Non-lead stabilized, fungus resistant, 105C rated automotive insulation designed to meet the performance criteria of SAE J1128. Information provided by Georgia Gulf Georgia Gulf became Axiall Corporation, which was later acquired by Westlake Plastics. This specific grade is discontinued. |