MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Santoprene® 101-55 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range of applications. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It is polyolefin based and completely recyclable.

Key Features:

  • UL listed: file #QMFZ2.E80017, Plastics - Component; file #QMFZ8.E80017, Plastics Certified For Canada - Component.
  • Although not NSF certified, this product has a Material Supplier Form on file with NSF to facilitate its evaluation for use in applications requiring NSF certification.
  • Recommended for applications requiring excellent flex fatigue resistance.
  • Excellent ozone resistance.
  • EU and China RoHS compliant.
Applications:
  • Automotive
    • Air Filter Gaskets
    • Air Induction System Ducts
    • Plugs, Bumpers, Grommets, Clips
    • Seals and Gaskets
  • Consumer
    • Electronics
  • Industrial
    • Seals and Gaskets
Uses:
  • Appliance Components
  • Consumer Applications
  • Gaskets
  • Automotive Applications
  • Diaphrams
  • Seal s
  • Automotive Under the Hood
  • Electrical Parts
  • Tubing
Processing Method: Coextrusion, Injection Molding, Profile Extrusion, Extrusion, Multi Injection Molding and Sheet Extrusion

Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South America

Information provided by ExxonMobil

Key Words: EU 2003/11/EC; RoHS Compliant; UL JMLU2; UL QMFZ2; UL QMFZ8
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.970 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 590.0787 in; ASTM D2240
 62
@Treatment Temp. 150 °C,
Time 605000 sec
in Air; ASTM D573
Tensile Strength at Break 754 psiAcross Flow; ASTM D412
 4.48 MPa
@Treatment Temp. 150 °C,
Time 605000 sec
in Air; ASTM D573
Tensile Stress at Strain 305 psi
@Strain 100 %
Across Flow; ASTM D412
Elongation at Break 400 %Across Flow; ASTM D412
 452 %
@Treatment Temp. 150 °C,
Time 605000 sec
in Air; ASTM D573
Tear Strength 91.4 pli73°C, Die C, Across Flow; ASTM D624
Compression Set 22 %
@Temperature 70.0 °C,
Time 79200 sec
Type 1; ASTM D395
 38 %
@Temperature 125 °C,
Time 252000 sec
Type 1; ASTM D395
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.41.93 mm; ASTM D150
Dielectric Strength 690 V/mil2.03 mm; ASTM D149
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 275 °CSAE J2236
Brittleness Temperature -76.0 °FASTM D746
UL RTI, Electrical 90.0 °CUL 746
UL RTI, Mechanical with Impact 90.0 °C
@Thickness 1.00 mm
UL 746
 90.0 °C
@Thickness 1.50 mm
UL 746
 95.0 °C
@Thickness 3.00 mm
UL 746
Flammability, UL94 HB
@Thickness 1.00 mm
 HB
@Thickness 1.50 mm
 HB
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 175 - 230 °C
Rear Barrel Temperature 350 °F
Middle Barrel Temperature 360 °F
Front Barrel Temperature 360 °F
Nozzle Temperature 370 - 430 °F
Die Temperature 390 °FExtrusion
Melt Temperature >= 385 °FExtrusion
 380 - 450 °FProcessing
Mold Temperature 50.0 - 125 °FProcessing
Drying Temperature 180 °F
Dry Time 3 hour
Moisture Content 0.080 %
Back Pressure 50.0 - 100 psiProcessing
 725 - 2900 psiExtrusion
Clamp Pressure 6000 - 10000 psi
Vent Depth 0.00100 in
Cushion 0.125 - 0.250 in
Screw Speed 100 - 200 rpm
 
Descriptive Properties
ColorBlack
FormPellets
Injection RateFast
Maximum Regrind %20
Screw Compression Ratio2:1 - 2.5:1
Screw L/D Ratio16:1 - 20:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 101-64 Thermoplastic Elastomer
EMS-Grivory Grilon® BG-50 PA6-GF50
ExxonMobil Santoprene® 101-45W255 Thermoplastic Elastomer
ExxonMobil Santoprene® 111-45 Thermoplastic Elastomer
ExxonMobil Santoprene® 101-87 Thermoplastic Elastomer

PADVA039 / 22729

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.