System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Cossa Polimeri ESTAPROP H 1280 T8 Polypropylene, 40% Mineral Filled
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
;
Polypropylene, Mineral Reinforced
Material Notes:
PP homopolymer 40% mineral filler
Excellent physical and mechanical characteristics, good surface appearance
Information provided by Cossa Polimeri S.r.l.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.25
g/cc
0.0452
lb/in³
ASTM D 792
Linear Mold Shrinkage
0.010
-
0.012
cm/cm
0.010
-
0.012
in/in
ASTM D 955
Melt Flow
12
g/10 min
@Load 2.16 kg,
Temperature 230 °C
12
g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D 1238
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
21.0
MPa
3050
psi
ASTM D 638
Tensile Strength, Yield
25.0
MPa
3630
psi
ASTM D 638
Elongation at Break
20 %
20 %
ASTM D 638
Tensile Modulus
4.10
GPa
595
ksi
ASTM D 638
Flexural Modulus
3.80
GPa
551
ksi
ASTM D 790
Izod Impact, Notched
0.150
J/cm
@Temperature -20.0 °C
0.281
ft-lb/in
@Temperature -4.00 °F
ASTM D 638
0.200
J/cm
@Temperature 0.000 °C
0.375
ft-lb/in
@Temperature 32.0 °F
ASTM D 638
0.300
J/cm
@Temperature 23.0 °C
0.562
ft-lb/in
@Temperature 73.4 °F
ASTM D 256
Thermal Properties
Metric
English
Comments
Deflection Temperature at 1.8 MPa (264 psi)
72.0
°C
162
°F
120°C/hr; ASTM D 648
Vicat Softening Point
97.0
°C
@Load 5.00 kg
207
°F
@Load 11.0 lb
50°C/hr; ASTM D 1525
Flammability, UL94
HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Aclo Accutech Polypropylene CP0435G43CV Copolymer Glass Reinforced Coupled
LG Chemical LUPOL GP-3152F General Purpose Polypropylene, 15% Mineral Fillers, High Impact, Flame Retardant
Overview of materials for Polypropylene with 30% Glass Fiber Filler
RTP Company RTP 102 GB 25 Polypropylene (PP) Glass Fiber 15% - Glass Bead 25%
Addiplast Addilene H 490 M40F Flame Retardant Polypropylene, 40% Mineral Filled
PCOSSA807 / 156397
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.