MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Danquinsa EMULTROL® E-166 Adhesive
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: EMULTROL E-166 is a high quality, aqueous tackifier emulsion, which results in very good adhesion properties, even on non-polar substrates and polymer-bound cardboard surfaces. EMULTROL E-166 is well applicable in acrylate, PVAc, EVA, SBR, NBR and polyurethane dispersions. For EMULTROL E-166 especially the adhesion properties and high surface tack properties have been adjusted. This tackifier emulsion has also an excellent wetting effect on silicone coated transfer surfaces. The tackifier emulsion is characterized by good oxidation and UV resistances. As EMULTROL E-166 is produced very finely dispersed, it results in a very good storage stability and a good homogeneity in the adhesive formulations. At the adhesive formulation it is important to adjust the right pH-value for a good compatibility with this resin emulsion. The pH-value can be set accordingly in the formulations with alkaline additives as for e.g. caustic soda or ammonia. At a too high alkaline pH-value or at a too acid formulation of the formulations, a coagulation of the adhesive formulation can occur.

Application: EMULTROL E-166 is an optimal tackifier emulsion for the equipment of aqueous adhesion and label adhesives. Construction adhesives, which have to present a long open time and for which an adhesion improvement for different substrates has to be carried out, are also modified with such tackifier emulsions. EMULTROL E-166 is all over used in adhesive formulations, where a very good adhesion is necessary on difficult synthetic foils, which have to be bonded. The product is also used for adhesive tape coatings and self-adhesive equipments of textiles and synthetic foils.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.01 - 1.03 g/cc
pH 6.5 - 8.5
Viscosity 2000 - 5000 cPRV8, Spindle 3, 50 rpm
Storage Temperature 10.0 - 25.0 °C
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 30[mg KOH/g], residium
 
Thermal PropertiesOriginal ValueComments
Boiling Point 100 °C
Softening Point 68.0 - 75.0 °CResidue soft point
Glass Transition Temp, Tg 5.00 - 10.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
 
Descriptive Properties
Active matter contents57-59%
AspectWhitish liquid
CompositionHighly stable esterified rosin resin emulsion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDANQ177 / 294597

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.