SUMILITERESIN® PR-1095 I is a powder novolac phenolic resin with modified high Tall Oil and a hexamine content of approximately 7%. For Friction Material: improves flexibility, friction coefficient, and creates a good feeling of braking. For Rubber Reinforcing: Low mooney viscosity, easy mixture, improves flexibility, and preferable for SBR compounds.Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp) |