MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Copper Alloy, UNS C18020, H02 Temper, Flat Products
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: 1/2 Hard

Fabrication Properties: Excellent Suitability – Soldering; Good Suitability – Capacity for Being Cold Worked, Capacity for Being Hot Formed

Common Fabrication Processes: Forming and Bending; Stamping

Typical Uses: Connector Components, Lead Frames

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.91 g/cc0.322 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 359 - 441 MPa52000 - 64000 psi
 400 MPa58000 psiTypical
Tensile Strength, Yield 331 - 407 MPa48000 - 59000 psi0.2% Offset
 372 MPa54000 psi0.2% Offset, Typical
Elongation at Break >= 10 %>= 10 %
Tensile Modulus 121 GPa17500 ksi
Modulus of Rigidity 45.36 GPa6579 ksiCalculated
Poissons Ratio 0.330.33
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000210 ohm-cm0.00000210 ohm-cm81% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.9 µm/m-°C
@Temperature 20.0 - 300 °C
9.40 µin/in-°F
@Temperature 68.0 - 572 °F
Thermal Conductivity 27.5 W/m-K191 BTU-in/hr-ft²-°F
Melting Point >= 1080 °C>= 1980 °F
Solidus 1080 °C1980 °F
 
Component Elements PropertiesMetricEnglishComments
Chromium, Cr 0.10 - 0.30 %0.10 - 0.30 %
Copper, Cu 99.1 - 99.8 %99.1 - 99.8 %As Balance
Silicon, Si <= 0.050 %<= 0.050 %
Tin, Sn 0.050 - 0.25 %0.050 - 0.25 %
Zinc, Zn 0.10 - 0.30 %0.10 - 0.30 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC18020x1 / 291613

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.