MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Encom Polymers EnLon 6630GFHS Nylon 66, 30% Glass Filled, Heat Stabilized, and Lubricated
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled; Nylon 66, Heat Stabilized

Material Notes: Appearance: Black, Natural or Colors

Processing Methods: Injection Molding

Applications: Automotive, Material Handling

Information provided by EnCom Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.39 g/cc1.39 g/ccASTM D792
Filler Content 30 %30 %
Maximum Moisture Content 0.0200.020
Linear Mold Shrinkage, Flow 0.0030 - 0.0060 cm/cm
@Thickness 3.20 mm
0.0030 - 0.0060 in/in
@Thickness 0.126 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 138 MPa20000 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
Flexural Modulus 7.586 GPa1100 ksiASTM D790
Izod Impact, Notched 0.690 J/cm1.29 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 232 °C450 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 277 - 299 °C530 - 570 °F
Middle Barrel Temperature 277 - 299 °C530 - 570 °F
Front Barrel Temperature 266 - 277 °C510 - 530 °F
Nozzle Temperature 277 - 299 °C530 - 570 °F
Melt Temperature 282 - 304 °C540 - 580 °F
Mold Temperature 65.6 - 104 °C150 - 220 °F
Drying Temperature 73.9 - 93.3 °C165 - 200 °F
Dry Time 3.00 - 6.00 hour3.00 - 6.00 hour
Back Pressure 0.138 - 0.414 MPa20.0 - 60.0 psi
Screw Speed 40 - 120 rpm40 - 120 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENCOM052 / 266066

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.