MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LyondellBasell Hostacom M2 N42 LG84014 Polypropylene, Mineral Reinforced  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Mineral Reinforced

Material Notes: Hostacom M2 N42 LG84014 is a mineral filled PP homopolymer with low melt flow rate. Product is UL listed. Applications: White Goods

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ISO 1183-1A
Melt Flow 7.0 g/10 min
@Load 5.00 kg,
Temperature 230 °C
7.0 g/10 min
@Load 11.0 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 37.0 MPa5370 psiISO 527-1,-2
Elongation at Yield 5.0 %5.0 %ISO 527-1,-2
Tensile Modulus 3.00 GPa435 ksiISO 527-1,-2
Flexural Modulus 3.10 GPa450 ksiTech.A; ISO 178/A1
Charpy Impact Unnotched 5.50 J/cm²26.2 ft-lb/in²ISO 179-1/1eU
Charpy Impact, Notched 0.400 J/cm²
@Temperature 23.0 °C
1.90 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 115 °C239 °Funannealed; ISO 75B-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 68.0 °C154 °Funannealed; ISO 75A-1,-2
Vicat Softening Point 95.0 °C203 °FB50; ISO 306
 
Descriptive Properties
Processing MethodInjection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Hostacom M2 N42 L356015 Polypropylene, Mineral Reinforced
LyondellBasell Hostacom M2 N01 L304698 Polypropylene, Mineral Reinforced
LyondellBasell Hostacom M2 N01 102942 Polypropylene with 20% Talc Filler
LyondellBasell Hostacom M2 R18 301105 Polypropylene, Mineral Reinforced
LyondellBasell Hostacom M4 U02 102943 BLK Polypropylene, Mineral Reinforced

PEQT8013 / 219649

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.