MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

(Viewing data as-entered. Click here to return)
Cookson Group Plaskon® SMT-B-1LAR Low Alpha, Fast Curing Molding Compound for PBGAs  (discontinued **)
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Molding Compound

Material Notes: This material is an epoxy molding compound optimized specifically for grid arrays (BGA/LGA) requiring low alpha particle count. It has the same unique resin system as the SMT-B-1, which minimizes warpage and enables trouble-free molding onto rigid and flexible laminate substrates. An all spherical filler system ensures outstanding moldability especially with automated and conventional molding systems. Minimal dimensional change after molding, post bake and subsequent solder treatment make this compound an excellent choice for grid array applications.

Features:

  • Minimal warpage
  • Low stress
  • Low viscosity
  • Low alpha particle content
  • Outstanding high temperature flexural strength

Information provided by Cookson Electronics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.88 g/cc
Viscosity 5000 cP
@Temperature 175 °C
Automatic orifice Viscosity
Linear Mold Shrinkage 0.00050 cm/cm
Spiral Flow 100 cmat 177°C and 1000 psi
Ash 77 %
Storage Temperature <= 5.00 °CRecommended
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 75Cull hot, 90 sec @ 175°C
Flexural Strength 15650 psi
 6400.5 psi
@Temperature 215 °C
Flexural Modulus 1.991e+6 psi
 853400 psi
@Temperature 215 °C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cm
@Temperature 22.0 °C
Dielectric Constant 3.7
@Frequency 1000 Hz
Dielectric Strength 400 V/mil
Dissipation Factor 0.0021
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.0 µm/m-°C
@Temperature 20.0 °C
Alpha 1
 56.0 µm/m-°C
@Temperature 20.0 °C
Alpha 2
Thermal Conductivity 0.700 W/m-K
Glass Transition Temp, Tg 222 °C
Flammability, UL94 V-0
@Thickness 3.17 mm
Oxygen Index 34 %
 
Processing PropertiesOriginal ValueComments
Mold Temperature 170 - 185 °C
Back Pressure 750 - 1000 psi
Cure Time 0.000 - 4.00 hour
@Temperature 175 °C
Post mold
 60.0 - 90.0 sec
@Temperature 177 °C
Gel Time 0.150 minRam follower, at 177°C and 1000 psi
Shelf Life 0.0670 Monthat 35°C, <40% loss of spiral flow
 0.167 Monthat 21°C, <40% loss of spiral flow
 24.0 Monthat 5°C, <40% loss of spiral flow
 
Descriptive Properties
Alpha Particle Count<0.001 counts/cm2/hr
Hydrolyzable Cl<1 ppm
Preheat Temperature90-100°C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPLASK007 / 56297

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.