MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Thermal Ceramics FireMaster Marine Blanket
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: FireMaster Marine Blanket is a lightweight, non-combustible mat that is produced from a calcium- magnesium-silicate raw material. There are no organic binders present in this mechanically needled mat producing no smoke or flame during a fire condition and maintains good surface integrity and strength. This fiber technology is soluble within the human body and provides excellent thermal and acoustic properties.

Features:

  • UL classified R8418, Non-combustibility per ISO 1182
  • US Coast Guard, DNV, and ABS approved for structural fire protection of IMO high speed craft and SOLAS commercial vessels
  • DNV and Lloyds approved for off-shore platform hydrocarbon bulkhead and deck applications
  • Up to 50% weight and installed savings over mineral wool
  • Aluminum and steel bulkhead and deck systems: A30, A60, and H60 Bulkhead and Deck structural insulation
  • Mechanical abuse and oil spray protection facings available
  • Inert and resistant to mold growth and attack of vermin
  • Applications:

  • A30 - Aluminum Bulkhead/Decks
  • A60 - Aluminum Bulkhead/Decks
  • A30-Steel Bulkhead/Decks
  • A60-Steel Bulkhead/Decks
  • H60-Steel Bulkhead/Decks
  • Marine fire doors
  • Marine exhaust pipes
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 0.0960 g/ccAvailable in multiple densities
     0.128 g/ccAvailable in multiple densities
     0.160 g/ccAvailable in multiple densities
     0.192 g/ccAvailable in multiple densities
    Loss On Ignition 0.00 %
     
    Thermal PropertiesOriginal ValueComments
    Thermal Conductivity 0.400 BTU-in/hr-ft²-°F
    @Temperature 260 °C
    10 pcf; ASTM C201
     0.400 BTU-in/hr-ft²-°F
    @Temperature 260 °C
    12 pcf; ASTM C201
     0.420 BTU-in/hr-ft²-°F
    @Temperature 260 °C
    8 pcf; ASTM C201
     0.460 BTU-in/hr-ft²-°F
    @Temperature <=260 °C
    6 pcf; ASTM C201
     0.710 BTU-in/hr-ft²-°F
    @Temperature 538 °C
    12 pcf; ASTM C201
     0.800 BTU-in/hr-ft²-°F
    @Temperature 538 °C
    10 pcf; ASTM C201
     0.880 BTU-in/hr-ft²-°F
    @Temperature 538 °C
    8 pcf; ASTM C201
     1.02 BTU-in/hr-ft²-°F
    @Temperature <=538 °C
    6 pcf; ASTM C201
     1.30 BTU-in/hr-ft²-°F
    @Temperature 816 °C
    10 pcf; ASTM C201
     1.41 BTU-in/hr-ft²-°F
    @Temperature 816 °C
    12 pcf; ASTM C201
     1.44 BTU-in/hr-ft²-°F
    @Temperature 982 °C
    12 pcf; ASTM C201
     1.53 BTU-in/hr-ft²-°F
    @Temperature 816 °C
    8 pcf; ASTM C201
     1.63 BTU-in/hr-ft²-°F
    @Temperature 982 °C
    10 pcf; ASTM C201
     1.78 BTU-in/hr-ft²-°F
    @Temperature <=816 °C
    6 pcf; ASTM C201
     1.95 BTU-in/hr-ft²-°F
    @Temperature 982 °C
    8 pcf; ASTM C201
     2.28 BTU-in/hr-ft²-°F
    @Temperature <=982 °C
    6 pcf; ASTM C201
    Melting Point 2327 °F
    Maximum Service Temperature, Air 1832 °F
    Flammability Test 0.00Flame Spread
     0.00Smoke Developed
     0.00Fuel Contributed
    Shrinkage 2.0 %
    @Temperature 538 °C,
    Time 86400 sec
     3.0 %
    @Temperature 982 °C,
    Time 86400 sec
     
    Component Elements PropertiesOriginal ValueComments
    CaO 25 - 35 %
    MgO 4.0 - 7.0 %
    Other 1.0 %
    SiO2 60 - 70 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Armacell ArmaFORM® FR100 PET foam core
    Carlisle 201LL Carbon-Carbon Composite
    DIAB Rigid Foam IPN 20-649 Type 1
    DuPont Mobility and Materials Vespel® SF-0920 Polyimide Foam, Low Density
    General Plastics LAST-A-FOAM® FR-3703 Polyurethane Foam

    CTHERM116 / 2436

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.