MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Edinburg Plastics HTT605 PA 6 Impact Modified
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Impact Grade

Material Notes: Appearance: General Purpose All Colors

Processing Methods: Injection

Applications: General Purpose

Information provided by Edinburg Plastics, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.07 g/ccASTM D792-91
Linear Mold Shrinkage 0.0090 - 0.015 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 6000 psiASTM D638
Elongation at Break 150 %ASTM D638
Flexural Yield Strength 8000 psiASTM D790
Flexural Modulus 235000 psiASTM D790
Izod Impact, Notched 22.0 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 52.0 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 221 - 238 °C
Middle Barrel Temperature 260 - 277 °C
Front Barrel Temperature 277 - 293 °C
Nozzle Temperature 243 - 266 °C
Melt Temperature 243 - 271 °C
Mold Temperature 43.0 - 88.0 °C
Drying Temperature 79.0 °C
Dry Time 2.00 - 24.0 hour
Moisture Content <= 0.20 %
Dew Point >= -40.0 °F
Back Pressure 40.0 - 100 psiLower is better
Screw Speed 30 - 70 rpmLower is better

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ensinger Tecamid® HS Nylon (PA)
Edinburg Plastics HGT605 PA 6 Impact Modified
Global EPP PA 6C HS BLUE Cast Polyamide 6 + UV and Heat Stabilizers
Global Atron 602 IM Natural Nylon 6 Impact Modified
Eurotec® Tecomid® NA40 NL IL PA 6.6 impact modified

PEDIN035 / 183538

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.