MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Trelleborg Emerson & Cuming Eccobond® 45LV Two-Component General Purpose Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Emerson & Cuming 45LV Eccobond® Two-Component General Purpose Epoxy Adhesive
Low viscosity, filled, general purpose, room temperature curing, epoxy adhesive and sealant. Flexibility can be adjusted by the amount of Catalyst 15 used. Convenient mix ratio. Good impact resistance. Excellent adhesion to metal, glass and plastic substrates. Mix Ratio of 100:25 to 100:100 (Cat 15 LV variation). Bonding Type: Epoxy

The Eccobond® product line is now a part of Henkel; this specific grade is discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 - 1.43 g/cc0.0444 - 0.0517 lb/in³
Viscosity 25000 cP
@Temperature 25.0 °C
25000 cP
@Temperature 77.0 °F
Mixed
 
Mechanical PropertiesMetricEnglishComments
Adhesive Bond Strength 16.5 MPa2400 psi
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min24.0 hour
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEMERS49 / 35741

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.