MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Solvay MTM® 49-3 Epoxy Prepreg with 42% CF2115 Carbon Fabric
Categories: Polymer; Thermoset; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: MTM49-3 is an 80 to 160°C (176 to 320°F) curing, toughened epoxy pregpreg resin system developed specifically for the manufacture of components. MTM49-3 pregregs exhibit excellent ambient and hot mechanical performance combined with good impact resistance after only moderate cure cycles making them ideal for use in the motorsport industry.

Features & Benefits:

  • Autoclave and press curable
  • 60 days out life at 21°C (70°F)
  • 12 months storage at -18°C(0°F)
  • Versatile cure temperatures
  • 190°C Tg
  • Bonds directly to Nomex core in body type applications
Product Variants:
MTM49-3: High Tg and moderate toughness
MTM49-3B: Black pigmented variant of MTM49-3
MTM49-3BB: Black pigmented variant of MTM49-3 (higher pigment loading)
MTM49-3BD: Black dyed variant of MTM49-3

Property data reported for dry sample after cure cycle: 90 minutes at 135°C (275°F), 6.2 bar (90 psi). Data normalized to 48 vol% except for shear properties. CF2115 is a 200 g/m2 2x2 twill fabric with 6k M46J fibers

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.22 g/ccUnreinforced cured resin
Storage Temperature -18.0 °CResin
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 14800 psi90°; ASTM D3039
 58600 psi0°; ASTM D3039
Tensile Modulus 102 GPa90°; ASTM D3039
 104 GPa0°; ASTM D3039
Compressive Strength 370 MPa90°; SACMA SRM01R94
 400 MPa0°; SACMA SRM01R94
Compressive Modulus 87000 MPa90°; SACMA SRM01R94
 89000 MPa0°; SACMA SRM01R94
Shear Modulus 3.98 GPaIn-plane; ASTM D3518
Shear Strength 7280 psi0° Interlaminar; ASTM D2344
 12000 psiIn-plane; ASTM D3518
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 95.0 °CDMA E' onset Tg, 16 hrs at 80°C, dry
 <= 115 °Cwet
 140 °CDMA E' onset Tg, 90 mins at 135°C, dry
 <= 190 °Cdry
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 120 °C
Alternate Cure
 1.50 hour
@Temperature 135 °C
Recommended Cure
 4.00 hour
@Temperature 100 °C
Alternate Cure
 7.00 min
@Temperature 160 °C
Alternate Cure
 25.0 min
@Temperature 140 °C
Alternate Cure
Shelf Life 12.0 MonthResin

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay MTM® 49-3 Epoxy Prepreg with 42% CF1218 Carbon Fabric
Solvay CYCOM® 2020 Epoxy + T800-6K 2X2T Twill 200 Prepreg, without Post-Cure
Solvay CYCOM® 977-6 Epoxy Laminate with IM7 Unidirectional Tape
Hexcel® HexPly® EH 84 120°C Curing Epoxy Matrix, Intermediate Modulus 12k carbon UD tape 150 g/m2
Solvay CYCOM® 2040 Epoxy Prepreg Fabric with 6KT800-2X2T-200

PCYTED146e / 233298

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.