MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Avient Maxxam® NZ-218.G001 Polypropylene (PP), Calcium Carbonate Filled  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes:

Description/Features:

  • Calcium Carbonate Filled
PolyOne First Choice

Information provided by PolyOne Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.969 g/cc0.0350 lb/in³ASTM D792
Filler Content 10 %10 %Reinforcement Level
Linear Mold Shrinkage 0.011 - 0.015 cm/cm0.011 - 0.015 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9090ASTM D785
Tensile Strength, Yield 30.7 MPa4450 psiType 1 - Rigids, 2 in/min; ASTM D638
Elongation at Break 165 %165 %Type 1 - Rigids, 2 in/min; ASTM D638
Flexural Strength 37.9 MPa5500 psiASTM D790
Flexural Modulus 1.59 GPa230 ksiASTM D790
Izod Impact, Notched 0.374 J/cm
@Thickness 3.17 mm,
Temperature 23.0 °C
0.700 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Izod Impact, Unnotched 4.81 J/cm
@Thickness 3.17 mm,
Temperature 23.0 °C
9.00 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded Bars; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 92.8 °C199 °FAnnealed, 0.125 in bars; ASTM D648
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0590 in
All Colors

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Maxxam® DP-8973-2 Polypropylene (PP), Calcium Carbonate Filled
Avient Maxxam® 8435 Polypropylene (PP), Calcium Carbonate Filled
Avient Maxxam® GZ-215 S002-1000 Polypropylene (PP), Calcium Carbonate Filled
Avient Maxxam® MH-418.G001 Polypropylene (PP), Calcium Carbonate Filled
Avient Maxxam® MH-418.F001 Polypropylene (PP), Calcium Carbonate Filled

PH1PO2698 / 44684

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.