MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Vibrantz Technologies EG 4000 Display Device
Categories: Ceramic; Glass

Material Notes: Glass Type: Pb-B (Composite)
Typical Powder Form: VEG
Typical Application: Seal

Ferro's display sealing glasses and dielectrics are low-temperature lead glasses suitable for hermetic sealing and passivation of soda lime glass packages, including plasma display panels and tubes.

Information provided by Ferro Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 5.70 g/cc0.206 lb/in³
Particle Size 10 µm10 µm50% of particles
 <= 75 µm<= 75 µm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.60 µm/m-°C4.78 µin/in-°Fat Set Pt.
 8.15 µm/m-°C
@Temperature 260 °C
4.53 µin/in-°F
@Temperature 500 °F
Softening Point 350 °C662 °F
Transformation Temperature 295 °C563 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 400 °C752 °FTypical Firing Temperature; Typical Firing Time: 10 min.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borosilicate Glass
Colorite Polymers 7066 Non-Phthalate 66 Series Vinyl Compound
Corning Pyrex® 7740 Borosilicate Glass Sheet
Geon® Performance Solutions HC 8210 Polyvinyl Chloride, Rigid
Mo-Sci Corporation GL-0191 Soda-Lime Glass Spheres

CFERR12 / 826

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.