MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Niagara LaSalle 8620 Leaded Cold Finished Steel Bar
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 8000 Series Steel

Material Notes: Lead added to this grade increases parts production by some 25% with excellent finish and good tool life. Machining speeds are increased to 145 sfm and there are no adverse effects on properties. Readily carburized, the well balanced alloy content of this grade permits hardening to produce a strong, tough core and high case hardness.

Information provided by Niagra LaSalle Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.18 - 0.23 %0.18 - 0.23 %
Chromium, Cr 0.40 - 0.60 %0.40 - 0.60 %
Iron, Fe 96.545 - 97.87 %96.545 - 97.87 %as balance
Lead, Pb 0.15 - 0.35 %0.15 - 0.35 %
Manganese, Mn 0.70 - 0.90 %0.70 - 0.90 %
Molybdenum, Mo 0.15 - 0.25 %0.15 - 0.25 %
Nickel, Ni 0.40 - 0.70 %0.40 - 0.70 %
Phosphorus, P <= 0.035 %<= 0.035 %
Silicon, Si 0.15 - 0.35 %0.15 - 0.35 %
Sulfur, S <= 0.040 %<= 0.040 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Niagara LaSalle 8620 Cold Finished Steel Bar
AISI 8620 Steel, normalized, 13 mm (0.5 in.) round
AISI 8620 Steel, normalized, 50 mm (2 in.) round
AISI 8620 Steel, single quenched and tempered (150°C (300°F)), carburized
AISI 11L17 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round

NNIAL016 / 160306

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.