MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Kazanorgsintez PC-005 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Production Method: Obtained by means of polycondensation method.

Application: Intended for product manufacture by method of extrusion and die-casting.

Information Provided by Kazanorgsintez

Key Words: PC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 4.0 - 6.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
4.0 - 6.0 g/10 min
@Load 2.65 lb,
Temperature 572 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield >= 55.0 MPa>= 7980 psi2nd Grade
 >= 58.0 MPa>= 8410 psi1st Grade
 >= 60.0 MPa>= 8700 psiSuperior Quality
Elongation at Break >= 80 %>= 80 %2nd Grade
 >= 100 %>= 100 %Superior Quality, 1st Grade
Flexural Modulus 2.00 GPa290 ksi2nd Grade
 2.25 GPa326 ksiSuperior Grade, 1st Grade
Transverse Strength >= 80.0 MPa>= 11600 psi2nd Grade, at max sample load
 >= 90.0 MPa>= 13100 psiSuperior Quality, 1st Grade, at max sample load
Compressive Yield Strength >= 70.0 MPa>= 10200 psi1st Grade, 2nd Grade
 >= 76.0 MPa>= 11000 psiSuperior Quality
Izod Impact, Unnotched (ISO) 60.0 kJ/m²28.6 ft-lb/in²2nd Grade
 66.0 kJ/m²31.4 ft-lb/in²Superior Grade, 1st Grade
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant <= 3.1
@Frequency 1000 Hz
<= 3.1
@Frequency 1000 Hz
Superior Quality
Dielectric Strength >= 20.0 kV/mm>= 508 kV/inSuperior Quality
Dissipation Factor <= 0.0090
@Frequency 1000 Hz
<= 0.0090
@Frequency 1000 Hz
Superior Quality
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point >= 147 °C>= 297 °F
 
Optical PropertiesMetricEnglishComments
Yellow Index 1.6 - 2.2 %1.6 - 2.2 %Superior Grade
 1.0 - 3.5 %1.0 - 3.5 %1st Grade
Transmission, Visible 85 %85 %2nd Grade
 89 %89 %Superior Quality, 1st Grade
 >= 90 %>= 90 %Superior Grade, 1st Grade
 
Descriptive Properties
Amount of impurities [pcs]101st Grade
 5Superior Quality
Turbidity0.8Superior Grade, 1st Grade
 12nd Grade

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Network Polymers PC-1006
Mitsubishi Xantar® MX 2015 Polycarbonate
Iran Petrochemical (PCC) PC 3038 Polycarbonate
Iran Petrochemical (PCC) PC 0712 Polycarbonate
Global PC-1424 Standard Grade Polycarbonate

PKAZAN090 / 127409

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.