MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Amodel® HFZ A-4133L PPA, 33% glass fiber
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 30% Glass Fiber Reinforced

Material Notes: 33% glass fiber, high flow, fast cycle time, hot-water molds, lubricated

Amodel® HFZ A-4133 L polyphthalamide (PPA) is a 33% glass-reinforced, hot water moldable resin. Key properties include heat resistance, reduced outgassing and high strength and stiffness over a broad temperature range. It also displays low moisture absorption, excellent chemical resistance and excellent electrical properties.

Amodel® HFZ A-4133 L resin is ideal for automotive electrical and electronic applications, including connectors, sockets, switches and sensors. It is also a good choice for under-hood enclosures that protect critical control systems such as anti-lock brakes, traction control, steering, electronic engine control, transmission and chassis control units.

- Black: HFZ A-4133 L BK 324
- Natural: HFZ A-4133 L NT

Applications: Automotive Applications; Automotive Electronics; Automotive Under the Hood; Bobbins; Camera Applications; Cell Phones; Connectors; Electrical/Electronic Applications; General Purpose; Industrial Applications; Industrial Parts; Lawn and Garden Equipment; Machine/Mechanical Parts; Metal Replacement

Features: Chemical Resistant; Creep Resistant; Fast Molding Cycle; Good Dimensional Stability; Good Stiffness; High Flow; High Stiffness; High Strength; Hot Water Moldability; Low Moisture Absorption; Lubricated

Injection notes: Injection Pressure: 3 to 4 in/sec
Storage:
- Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding following the recommendations found in this datasheet and/or in the Amodel® processing guide.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.46 g/ccMethod A; ISO 1183
Water Absorption 0.26 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.010 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 180 MPaISO 527-2
Elongation at Break 1.8 %ISO 527-2
Tensile Modulus 12000 MPaISO 527-2
Flexural Strength 255 MPaISO 178
Flexural Modulus 11000 MPaISO 178
Izod Impact, Notched (ISO) 8.40 kJ/m²Type 1, Notch A; ISO 180
Izod Impact, Unnotched (ISO) 40.0 kJ/m²Type 1; ISO 180
Charpy Impact, Notched 8.20 kJ/m²Type 1, Edgewise, Notch A; ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D257
Surface Resistance 1.00e+16 ohmASTM D257
Dielectric Constant 3.7
@Frequency 1e+6 Hz
ASTM D150
 3.9
@Frequency 60 Hz
ASTM D150
Dielectric Strength 19.0 kV/mmASTM D149
Dissipation Factor 0.0060
@Frequency 60 Hz
ASTM D150
 0.016
@Frequency 1e+6 Hz
ASTM D150
High Voltage Arc Resistance to Ignition (HVAR) 0.00 - 10 secPLC 0; UL 746
Hot Wire Ignition, HWI 60 - 119 secPLC 1; UL 746
High Amp Arc Ignition, HAI >= 120 arcsPLC 0; UL 746
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/minPLC 0; UL 746
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 14.0 µm/m-°C
@Temperature 150 - 250 °C
ASTM E831
 20.0 µm/m-°C
@Temperature 0.000 - 90.0 °C
ASTM E831
CTE, linear, Transverse to Flow 63.0 µm/m-°C
@Temperature 0.000 - 90.0 °C
ASTM E831
 150 µm/m-°C
@Temperature 150 - 250 °C
ASTM E831
Melting Point 327 °CISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 310 °CUnannealed; ISO 75-2/A
Flammability, UL94 HB
@Thickness 0.800 mm
Glow Wire Ignition Temperature 800 °CIEC 60695-2-13
Glow Wire Flammability Index 800 °CIEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 318 - 324 °C
Front Barrel Temperature 327 - 332 °C
Melt Temperature 329 - 343 °CInjection
Mold Temperature 66.0 - 93.0 °C
Drying Temperature 120 °C
@Time 14400 sec
Moisture Content 0.030 - 0.060 %Injection
 
Descriptive Properties
AdditiveLubricant; Mold Release
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack; Natural Color
FormsPellets
ProcessingWater-Heated Mold Injection Molding
RoHS ComplianceYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4119 / 279919

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.