MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Evonik tert.-Butanol azetropic Liquid
Categories: Fluid

Material Notes: CAS No: 75-65-0

Properties: Tert.-Butanol is a colorless liquid which solidifies at room temperature. TBA is miscible with nearly all organic solvents (alcohol, ethers, ketones, esters and hydrocarbons) and water, too. TBA and water form an azeotropic mixture having a water content of 11.75%. In contrast to pure tert.-Butanol, the azeotrope is liquid even at room temperature. With strong acids, decomposition can take place mainly to give isobutene. Tert.-Butanol is largely stable to oxidizing agents and halogens, it is non-corrosive. Vapors can form explosive mixtures with air. Concentrated vapors have an anaesthetic effect.anaesthetic effect.

Use: Tert.-Butanol is a starting material for the production of tert.-butyl peroxides as polymerization initators. TBA is used as an alkylating agent for aromatics and phenols for the production of tert.-butylaromatics and, for example, tert.-butyl Cresol; for the production of tert.butyl esters as precursors for antioxidants, phenolic resins, pharmaceutical products dn perfumes. Due to its good dissolving properties and also good solubility in polar and non-polar substance, TBA is outstandingly suitable as a solvent and as a solubiliser, for example in waterbased paints, for the dewaxing of oils and as denaturing agent for Ethanol.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.803 g/cc0.0290 lb/in³relative
Viscosity <= 3.6 cP
@Temperature 30.0 °C
<= 3.6 cP
@Temperature 86.0 °F
Molecular Weight 74.12 g/mol74.12 g/mol
Vapor Pressure  23.4 bar
@Temperature 10.0 °C
17600 torr
@Temperature 50.0 °F
 46.4 bar
@Temperature 20.0 °C
34800 torr
@Temperature 68.0 °F
 86.7 bar
@Temperature 30.0 °C
65000 torr
@Temperature 86.0 °F
 153.9 bar
@Temperature 40.0 °C
115400 torr
@Temperature 104 °F
 260.9 bar
@Temperature 50.0 °C
195700 torr
@Temperature 122 °F
 424.9 bar
@Temperature 60.0 °C
318700 torr
@Temperature 140 °F
 
Chemical PropertiesMetricEnglishComments
Total Acid Number <= 0.010<= 0.010[mg KOH/g]; DIN EN ISO 2114
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 14
@Temperature 30.0 °C
14
@Temperature 86.0 °F
 
Thermal PropertiesMetricEnglishComments
Heat of Vaporization 577.8 J/g248.6 BTU/lbat bp
Specific Heat Capacity 3.19 J/g-°C
@Temperature 30.0 °C
0.762 BTU/lb-°F
@Temperature 86.0 °F
Melting Point -4.40 °C24.1 °F
Boiling Point 79.9 °C
@Pressure 0.1013 MPa
176 °F
@Pressure 14.69 psi
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.381.38
 
Descriptive Properties
Color<10DIN ISO 6271
Content<0.25%sec.-Butanol
 >87.25%TBA
 11.6-12.6%Water

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIL950 / 197154

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.