AMC™ 8592 is a chopped carbon fiber reinforced engineered structural composite molding compound. It is easily moldable and provides parts that are high strength, fatigue resistant, with high heat resistance and a low density. The carbon fiber is PAN based 12K tow.- Form = Rolled, Festooned Sheet
- Carbon Fiber Content = 55% nominal