MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

(Viewing data as-entered. Click here to return)
Taiwan PU CPU-42-BC30A-A/B Polyurethane Potting Compound
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Key features:
  • Halogen free
  • Flame retardant
  • Soft grade and can absorb vibration
  • Highly transparent sealing material
  • Good at blocking moisture
  • Great repairability
Description: The polyurethane potting compounds (CPU-42-BC30A-A/B and CPU-42-BC30D-A/B) are transparent two-component materials for electrical device and housing. The polyurethane potting compounds can also be used to cast for other suitable products.

Advantage:
Solvent-free (100% solid content)
Great electrical characteristics
Low initial viscosity after mixing (The performance is compared to solvent-free two component casting resin)
The reaction of mixture starts at room temperature (The reaction is speeded up at higher temperature)

Information provided by Taiwan PU Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.912 - 1.012 g/ccPart A
 1.005 - 1.105 g/ccPart B
Viscosity 280 - 400 cPPart B
 550 - 910 cPPart A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 31
@Time 605000 sec
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 V-2
@Thickness 1.80 mm
 
Processing PropertiesOriginal ValueComments
Pot Life 35.0 - 45.0 minViscosity increases to 50,000 cps
 
Descriptive Properties
AppearanceLight yellow liquidPart A
 Light yellow liquidPart B
CompositionModified polyisocyanatePart B
 PolyolPart A
Mixing ratio100:70Part A: Part B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTAIWPU025 / 305755

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.