Moplen EP340S is a heterophasic copolymer used in injection molding. This grade is nucleated and characterized by a good processability combined with a medium stiffness-impact balance Moplen EP340S is typically used in crates, house wares and opaque containers. Applications : Crates, House wares, Opaque Containers.Information provided by LyondellBasell. |