MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
KKPC KOSYN KBR 31 Polybutadiene Rubber (High cis BR)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Polybutadiene Rubber (High cis BR)

Characteristics: KBR 31 contains an aromatic oil additive. Polybutadiene Rubber (BR), which has three kinds of bond structure of cis-1,4, trans-1,4, vinyl, is simple polymer made from 1,3-butadiene by solution polymerization, and it is classified to High cis BR and Low cis BR according to the cis-1,4 content. High cis BR containing over 94% cis-1,4 is superior in abrasion resistance, elasticity, age resistance and water resistance. As the secondary transition temperature is about -100? low, it is most widely utilized together with SBR.

Applications: Conveyor belting, tires (superior for snow tire tread).

Additional Notes:
Extender Oil: 37.5; Aromatic
Stabilizer: Non-Polluting
cis-1,4 Contents: 95%
Volatile Matter: 0.3%
Ash Content: 0.1%

This product is so sensitive to sunlight and humidity that it can be tarnished and caused deterioration of quality if exposed. It is recommended to store it in cool and shady area lest it should be exposed to direct sunlight. Do not expose to incompatible materials or contaminants.

Data provided by Korea Kumho Petrochemical Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.930 g/ccNot Compounded
Mooney Viscosity 35
@Temperature 100 °C
Raw; ML1+4
 71
@Temperature 100 °C
Compounded; ML1+4; KOSYN KBR31 137.5, ZnO 3, Stearic Acid 2, HAF Black (IRB#6) 82.5, Accelerator TBBS 1.24, Sulfur 1.5 Total: 227.7
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 57Cured; JIS-A
Tensile Strength, Ultimate 192 kg(f)/cm²Cured
Elongation at Break 640 %Cured
300% Modulus 82.0 kg(f)/cm²
@Strain 300 %
Cured
Rebound 47 %ASTM
Flex Crack Resistance 6000De Mettia Flexometer Cut Growth: 2mm --> 15mm, Flexes
Tear Strength 71.0 kg(f)/cmB-type
Abrasion 0.0040Akron type Tester (cc/1000rev)
Compression Set 4.0 %Permanent Set
 13 %
@Temperature 70.0 °C
70°C / 22 hrs, 25%, def

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow SE BR-1220L Stereospecific high cis-1,4 Polybutadiene (BR)
Dow SE BR-1220M Stereospecific high cis-1,4 Polybutadiene (BR)
Synthos BUNA™ cis 132 Schkopau High-cis Polybutadiene Rubber (PBR)
Dow SE BCP 817 Stereospecific high cis-1,4 Polybutadiene (BR)
Dow SE BR-1203H Stereospecific high cis-1,4 Polybutadiene (BR)

PKKPC26 / 48757

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.