MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Loxim 340 01HB Nylon 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 40% Glass Fiber Filled; Nylon 6, Glass Fiber Filled, Flame Retardant

Material Notes:

Information provided by Loxim Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.50 g/ccASTM D792
Linear Mold Shrinkage 0.0020 cm/cmASTM D1299
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 180 MPaASTM D683
Elongation at Break 2.0 - 3.0 %ASTM D638
Flexural Modulus 9500 MPaASTM D790
Izod Impact, Notched 180 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 210 °CASTM D1525, HDT Method B
Flammability, UL94 HB
@Thickness 1.60 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Reny® 1022H Polyamide
NYCOA 27/300I Glass Filled Nylon 6
Nurel Engineering Polymers Promyde® B30 P2 G50 PA 6, Dry, 50% Glass Reinforced, Injection Molded and Heat Stabilized
Niche Polymer PA6GF50BK Nylon 6, 50% Glass Fiber Filled
Mitsubishi Reny® 2041 Polyamide

PLOXIM034 / 121368

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.