MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SCG Chemicals C2785XXX PVC Wire & Cable Compound
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Wire and Cable Grade

Material Notes: C2785XXX is PVC compound product with any color for using in wire and cable application product. The formulation is designed for Insulation 70 °C rated cable which give good process ability by extrusion.

Applications: 70 °C Rated for Insulation cable.

Features: Good process ability. Good surface of product. Non heavy metal.

Information provided by SCG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 - 1.23 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 70 - 73
@Time 10.0 sec
ASTM D2240
Tensile Strength 33.0 - 55.0 kg(f)/cm²JIS K6723
Elongation at Break 392 - 419 %JIS K6723
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 8.00e+12 - 1.60e+13 ohm-cmJIS K6723
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 70.0 °CInsulation Rating
 
Descriptive Properties
AppearancePellet
Heat Stability390-400 minTPC Method @ 180°C
Retention of Elongation at Break (%)90-95JIS K6723. Aging @ 80°C x 168 hrs.
Retention of Tensile Strength (%)94-97JIS K6723. Aging @ 80°C x 168 hrs.
Weight Loss (%)0-0.5JIS K6723. Aging @ 80°C x 168 hrs.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSCGC794 / 278051

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.