Physical Properties | Metric | English | Comments |
---|
Specific Gravity | 1.35 g/cc | 1.35 g/cc |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Shore A | 88 | 88 |
| 76 @Treatment Temp. 23.0 °C, Time 252000 sec | 76 @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 79 @Treatment Temp. 23.0 °C, Time 252000 sec | 79 @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 88 @Treatment Temp. 23.0 °C, Time 252000 sec | 88 @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 89 @Treatment Temp. 100 °C, Time 252000 sec | 89 @Treatment Temp. 212 °F, Time 70.0 hour |
| 89 @Treatment Temp. 100 °C, Time 252000 sec | 89 @Treatment Temp. 212 °F, Time 70.0 hour |
| 92 @Treatment Temp. 100 °C, Time 252000 sec | 92 @Treatment Temp. 212 °F, Time 70.0 hour |
| 94 @Treatment Temp. 100 °C, Time 252000 sec | 94 @Treatment Temp. 212 °F, Time 70.0 hour |
| 95 @Treatment Temp. 125 °C, Time 252000 sec | 95 @Treatment Temp. 257 °F, Time 70.0 hour |
| 95 @Treatment Temp. 125 °C, Time 252000 sec | 95 @Treatment Temp. 257 °F, Time 70.0 hour |
Tensile Strength | 17.39 MPa | 2522 psi |
| 12.329 MPa @Treatment Temp. 23.0 °C, Time 252000 sec | 1788.1 psi @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 14.937 MPa @Treatment Temp. 23.0 °C, Time 252000 sec | 2166.4 psi @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 16.380 MPa @Treatment Temp. 125 °C, Time 252000 sec | 2375.7 psi @Treatment Temp. 257 °F, Time 70.0 hour |
| 16.380 MPa @Treatment Temp. 125 °C, Time 252000 sec | 2375.7 psi @Treatment Temp. 257 °F, Time 70.0 hour |
| 17.319 MPa @Treatment Temp. 100 °C, Time 252000 sec | 2511.9 psi @Treatment Temp. 212 °F, Time 70.0 hour |
| 17.545 MPa @Treatment Temp. 23.0 °C, Time 252000 sec | 2544.7 psi @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 17.78852 MPa @Treatment Temp. 100 °C, Time 252000 sec | 2580.006 psi @Treatment Temp. 212 °F, Time 70.0 hour |
| 18.884 MPa @Treatment Temp. 100 °C, Time 252000 sec | 2738.9 psi @Treatment Temp. 212 °F, Time 70.0 hour |
Elongation, Ultimate | 110 % | 110 % |
| 30.04 % @Treatment Temp. 125 °C, Time 252000 sec | 30.04 % @Treatment Temp. 257 °F, Time 70.0 hour |
| 30.04 % @Treatment Temp. 125 °C, Time 252000 sec | 30.04 % @Treatment Temp. 257 °F, Time 70.0 hour |
| 69.96 % @Treatment Temp. 100 °C, Time 252000 sec | 69.96 % @Treatment Temp. 212 °F, Time 70.0 hour |
| 69.96 % @Treatment Temp. 100 °C, Time 252000 sec | 69.96 % @Treatment Temp. 212 °F, Time 70.0 hour |
| 79.97 % @Treatment Temp. 23.0 °C, Time 252000 sec | 79.97 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 89.98 % @Treatment Temp. 23.0 °C, Time 252000 sec | 89.98 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 89.98 % @Treatment Temp. 100 °C, Time 252000 sec | 89.98 % @Treatment Temp. 212 °F, Time 70.0 hour |
| 110 % @Treatment Temp. 23.0 °C, Time 252000 sec | 110 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
100% Modulus | 15.84 MPa | 2298 psi |
Tear Strength | 29.8 kN/m | 170 pli |
Compression Set | 10 % @Treatment Temp. 100 °C, Time 79200 sec | 10 % @Treatment Temp. 212 °F, Time 22.0 hour |
| 20 % @Treatment Temp. 100 °C, Time 79200 sec | 20 % @Treatment Temp. 212 °F, Time 22.0 hour |
|
Thermal Properties | Metric | English | Comments |
---|
Brittleness Temperature | -33.9 °C | -29.0 °F |
Shrinkage | -8.20 % @Treatment Temp. 100 °C, Time 252000 sec | -8.20 % @Treatment Temp. 212 °F, Time 70.0 hour |
| -0.100 % @Treatment Temp. 23.0 °C, Time 252000 sec | -0.100 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 0.60 % @Treatment Temp. 100 °C, Time 252000 sec | 0.60 % @Treatment Temp. 212 °F, Time 70.0 hour |
| 4.4 % @Treatment Temp. 100 °C, Time 252000 sec | 4.4 % @Treatment Temp. 212 °F, Time 70.0 hour |
| 16.5 % @Treatment Temp. 23.0 °C, Time 252000 sec | 16.5 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 29 % @Treatment Temp. 23.0 °C, Time 252000 sec | 29 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
|
Descriptive Properties |
---|
Color | Black |