MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

INEOS Styrolution Lustran® SAN CN27 Styrene Acrylonitrile (SAN)
Categories: Polymer; Thermoplastic; SAN Polymer; Styrene Acrylonitrile (SAN), Molded

Material Notes: SAN resin supplied in natural color and bead form for use in compounding applications. Applications: Compounding

Information provided by Styrolution.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³ASTM D 792
Melt Flow  15 g/10 min
@Load 3.80 kg,
Temperature 230 °C
15 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D 1238
 36 g/10 min
@Load 10.0 kg,
Temperature 220 °C
36 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D 1238

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution Lustran® SAN CN87 Styrene Acrylonitrile (SAN)
INEOS Styrolution Lustran® SAN CN88 Styrene Acrylonitrile (SAN)

PSTYR9839 / 216066

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.