MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Braskem CN8092 EVA Molding Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: CN8092 is an Ethylene-Vinyl Acetate copolymer (EVA) which has a molecular structure that provides easy processing, adhesion, resilience, low hardness, good moisture, and gas barrier properties. It is a non-halogen resin that has excellent thermal stability and a low content of oligomers, with low influence on organoleptic properties of the products. The melt properties of this resin allow processability in cast film and tubular film equipment. It contains antioxidant additives. Its applications include: base resin for production of compounds for cap liners in carbonated beverages; compounds; and master batches.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.934 g/ccASTM-D1505
Vinyl Acetate Content 15.5 %
Melt Flow 8.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM-D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 91ASTM-D2240
Hardness, Shore D 44ASTM-D2240
Tensile Strength at Break 17.0 MPaASTM-D638
Tensile Strength, Yield 4.70 MPaASTM-D638
Elongation at Break 720 %ASTM-D638
1% Secant Modulus 72.0 MPaASTM-D638
 
Thermal PropertiesOriginal ValueComments
Melting Point 90.0 °CASTM-D3418
Vicat Softening Point 62.0 °C
@Load 1.02 kg
ASTM-D1525
 
Processing PropertiesOriginal ValueComments
Melt Temperature 135 - 150 °CBlow Film Extrusion
 205 - 210 °CCast Film Extrusion
 225 °CExtrusion Coating
Die Opening 0.0800 - 0.100 cmBlow Film Extrusion
Blow-up Ratio (BUR) 2.0 - 3.0Blow Film Extrusion
Roll Temperature 25.0 °CChill, Cast Film Extrusion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Elvax® 660 Ethylene-Vinyl Acetate Copolymer Resin
Braskem TN2020 EVA General Film Copolymer
Westlake ELEVATE™ EF529 18.5% Ethylene Vinyl Acetate Copolymer
Arkema OREVAC® 9309 EVA Terpolymer
Braskem Evateno® 3019 PE EVA Foam Copolymer

PBRAS814 / 106660

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.