MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Solvay ThermalGraph® EWC-300X Fabric
Categories: Other Engineering Material; Composite Fibers

Material Notes: Description: ThermalGraph® Fabric EWC-300X is a pitch-based, high thermal conductivity woven fabric developed for thermal management applications. Due to the orthotropic nature of the weave, and the high longitudinal thermal conductivity of the fibers, biaxial thermal conductivity is achieved. Through-the-thickness thermal conductivity is enhanced by the weaving crimp. This product is easily prepregged and processed into a composite form. ThermalGraph EWC-300X is available as a plain weave fabric constructed from 4000 (4K) filament continuous pitch tows and as an eight harness satin fabric constructed from 2000 (2K) filament continuous pitch tows. Other filament counts and fabric styles can be provided on special order.

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.10 g/ccPlain Weave
 2.16 g/cc8 Harness Satin Weave
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 90.0 W/m-KPlain Weave, @ 60% Vf (cyanate matrix), warp and fill
 100 W/m-K8 Harness Satin Weave, @ 60% Vf (cyanate matrix), warp and fill
 250 - 350 W/m-KPlain Weave
 300 - 400 W/m-K8 Harness Satin Weave
 
Descriptive Properties
Carbon Assay8 Harness Satin Weave
 Plain Weave

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay ThermalGraph® EWC-600X Fabric
American Pine Wood
Applied Nanostructured Solutions PC/ABS - Carbon NanoStructure Chopped Fiber Composite
A-Glass Fiber, Generic
C-Glass Fiber, Generic

PCYTED071 / 180373

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.