MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Allyl cyanide
Categories: Fluid; Solvent

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.835 g/cc
@Temperature 20.0 °C
0.0302 lb/in³
@Temperature 68.0 °F
Viscosity 0.513 cP
@Temperature 20.0 °C
0.513 cP
@Temperature 68.0 °F
Dynamic Viscosity
Molecular Weight 67.091 g/mol67.091 g/mol
Vapor Pressure 0.019602 bar
@Temperature 20.0 °C
14.703 torr
@Temperature 68.0 °F
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 39.5 bar29600 torr
Critical Temperature 312 °C594 °F
Critical Density 0.253 g/cc0.00914 lb/in³
Critical Molar Volume 265 cm³/mol16.2 in³/mol
 
Thermal PropertiesMetricEnglishComments
Heat of Vaporization 511.4 J/g220.0 BTU/lb
Specific Heat Capacity 1.312 J/g-°C
@Temperature 25.0 °C
0.3136 BTU/lb-°F
@Temperature 77.0 °F
Vapor
Melting Point -86.5 °C-124 °F
Boiling Point 118.9 °C246.0 °F
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter16.0019
Antoine's Vapor Pressure B Parameter3128.75
Antoine's Vapor Pressure C Parameter-58.15
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
Critical Compressibility (Zc)0.22
Dipole moment (p/C.m)1.134E-27
Dynamic Viscosity Formulalog10 η=A(1/T-1/B)
Dynamic Viscosity Parameter A521.3
Dynamic Viscosity Parameter B252.03
Molar Heat Capacity (298K)88.041 J/mol-K
Molar Heat Capacity of Vapor a Parameter21.6857
Molar Heat Capacity of Vapor b Parameter0.257
Molar Heat Capacity of Vapor c Parameter-0.000191
Molar Heat Capacity of Vapor d Parameter1.228E-08
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

VORGS013 / 99407

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.