MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

DowAksa CFU23T Mid Weight Unidirectional Carbon Fabric
Categories: Carbon; Carbon Fiber/Carbon Fibre

Material Notes: DowAksa CFU20T is a medium weight, high tensile strength unidirectional carbon fabric. It easily wets out with CarbonBond™ 300-HT Saturant Resin System and can be installed using the “wet lay-up” technique. This fabric has excellent mechanical properties.

Applications: CFU20T Carbon Fabric is designed to fabricate on-site composite reinforcements to a variety of structures and substrates; Flexural and shear reinforcement of beams; In-plane and out-of-plane reinforcement of concrete and masonry walls; Column wrapping and reinforcement of slab; Structural steel applications.

Information provided by DowAksa.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.80 g/cc0.0650 lb/in³ISO 10119
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 4900 MPa710000 psiISO 10618
Elongation at Break 2.0 %2.0 %ISO 10618
Tensile Modulus 240 GPa34800 ksiISO 10618
 
Descriptive Properties
Weight20 oz/yd2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

EDOWAK972 / 287919

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.