VESTAKEEP® i4 G is a natural colored, high viscosity polyether ether ketone (PEEK) that is especially designed for long term implantable medical devices. This grade is often used for extrusion processing technologies. Dry properties listed below Industrial Sector: Medical Devices Processing: Injection molding, Extrusion Delivery form: Pellets, Granules Resistance to: Heat (thermal stability), Hydrolysis / hot water, Wear / abrasion, Fatigue resistance, Oil / fuels Conformity: Biocompatibility, Medical application Additives: Unfilled Special Characteristics: Semi-crystalline Regulatory: US Pharmacopeia Class VI conformity Color: Natural color Chemical Resistance: Acid resistance, Alkali resistance, Solvent resistance, Grease resistance, Hydrolytically stable, Oil resistance, Oxidation resistance, General chemical resistanceInformation provided by Evonik. |